• 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound
  • 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound
  • 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound
  • 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound
  • 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound
  • 125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound

125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound

CAS No.: N/a
Formula: N/a
EINECS: N/a
Molecular Principal Chain: Shielding
Color: White
Density: 1.52
Samples:
US$ 1000/kg 1 kg(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2023

Suppliers with verified business licenses

Rating: 5.0/5
Manufacturer/Factory
  • Overview
  • Product Description
Overview

Basic Info.

Model NO.
YT-6251
Transport Package
25kg/Bag
Specification
25KG/BAG
Trademark
LABEYOND
Origin
China

Product Description

Product Description

The product meets RoHS, REACH and other related environmental protection requirements. The material comply with EN 50618-2014, TUV 2pfg-1169 and IEC62930. Suitable for the insulation and sheath of solar cable.

Trade Mark and Appilcation 
 

Trade Mark Product Name Application
YT-6251 125ºC Silane-crosslinked halogen-free low-smoke flame-retardant polyolefin cable material Applicable for pressure-extrusion, for solar cable insulation

Performance Indexes

Can be customized according to customer's requirements.

Use Methods
1. Mixing: Mix the component A and component B evenly, add them into the hopper. If the color required, use the EVA base materials (the color masterbatch should be dried). The material should be use up within 2 hours after unpacking. (It can't be dried). The external water can' be brought in during the process.
2. Suggest to use equal distance & unequal depth, single thread screw.
3. Extrusion Temperature:
Zone 1 Zone 2 Zone 3 Zone 4 Neck Head
100±10 125±10 135±10 135±10 140±10 140±10
4. Double color cable: Color line can use component A and EVA base materials together, without or with a small numner of component B.
5. Pay-off speed: Without affecting of surface smoothness and perfirmance the faster, the better.
6. Crosslink:
Natural crosslink or water bath (Steam).
Natural Crosslink: Temperature 15-25ºC, crosslink will be finished around 7 days.
hen temperature is higher than 25ºC, crosslink will be finished around 3 days.
Water bath or Steam: should control the temperature arond 60-70 ºC in order to keep it from sticking together, it will finish about 4 hours. The thickness of the test piece is 1mm. It thickness >1mm, the crosslink time should be adjusted according to the actual situation. Full performance test, water bath (steam) 65ºC, more than 8 hours, to ensure the material is fully crosslinked.

Package, Transport and Storage
1. Package: Vacuum packed.
2. Transport: Can't be exposed to the sun or rain, or suffer mechanical damange.
3. Storage: Should be stacked on the backing plate in a clean and dry warehouse.
Valid Period: 12 months.
125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound125 Silane-Crosslinked Halogen-Free Low-Smoke Flame-Retardant Polyolefin Cable Compound